DIAMETRAL TENSILE STRENGTH, SHEAR BOND STRENGTH
DIAMETRAL TENSILE STRENGTH, SHEAR BOND STRENGTH
 
Document Language : English 
Abstract : The present study was done to evaluate the effect of addition of zirconia powder in 1%, 2% and 3% weight on a resin modified glass ionomer. SEM, diameteral tensile and shear bond strength to dentin were evaluated. It was found that, addition of 3% zirconia to the powder of glass ionomer resulted in a significant increase of diameteral tensile and shear bond strength of cement to dentin. SEM showed integration of zirconia powder between the glass powder and resin matrix resulted in improvement of strength properties. 
ISSN : 0 
Journal Name : Egyptian dental journal 
Volume : 52 
Issue Number : 4 
Publishing Year : 2006 AH
2006 AD
 
Article Type : Article 
Added Date : Monday, December 10, 2007 

Researchers

Researcher Name (Arabic)Researcher Name (English)Researcher TypeDr GradeEmail
محمد حامدHamed, Mohamed InvestigatorDoctorate 

Files

File NameTypeDescription
 DIAMETRAL TENSILE STRENGTH, SHEAR BOND STRENGTH.pdf pdf 

Download This Page

Back To Researches Page